Skip to content

Post-Tensioned Slab: How PT Floors Work in Commercial Buildings

Freshly finished concrete floor deck on a multistory building under construction with shoring below

A post-tensioned slab is concrete squeezed by steel tendons stretched after the pour, so a 9 inch flat plate can span about 30 feet. Crews stress the tendons 3 to 5 days after placement, and nobody should drill it blind.

Key takeaways

  • A 30 by 33 ft bay needs roughly a 9 in post-tensioned flat plate, a span-to-depth ratio near 44, per PTI Technical Note 22 (October 2023).
  • ACI 318 requires an average effective precompression of at least 125 psi in two-way post-tensioned slabs (Section 8.6.2.1), and the California State University peer-review guideline calls 150 to 175 psi optimum.
  • The CSU Guidelines for Post-Tensioned Concrete Structures (2018) require stressing within 3 to 5 days of the pour and prohibit drilling unless tendons are marked, x-rayed or photographed first.
  • The University of Houston Section 03 38 00 (rev. January 29, 2018) bars stressing below 3,000 psi and accepts measured elongations within 7 percent of calculated.
  • In a 2021 City of Tampa garage repair bid, fixing one broken tendon was priced at $500 to $4,470, with a $1,763.33 unit price from the low total bidder (bid tab 21-C-00036).

What is a post-tensioned slab and how do unbonded tendons work?

A post-tensioned slab is a cast-in-place concrete slab reinforced with high-strength steel strands that are tensioned after the concrete hardens, then locked off at anchors cast into the slab edges. In U.S. buildings the usual system is the unbonded single-strand tendon: a 270,000 psi strand (ASTM A416, per UH Section 03 38 00) coated in corrosion-inhibiting grease inside a plastic sheath, so the strand never bonds to the concrete.

Before the pour, crews drape each tendon high over the columns and low at midspan. When the jack pulls the strand at the stressing anchor, the curved tendon pushes up on the slab between supports and squeezes it lengthwise. That upward push carries part of the dead load, which is why the slab can be thinner than a rebar-only slab. CSU’s guideline asks designers to balance at least 65 percent and no more than 125 percent of the concrete weight.

Post-tensioned slab section with draped tendon profile Two interior spans of a 9 inch post-tensioned flat plate on columns at 30 feet. The unbonded tendon runs high over the columns and low at midspan, with a stressing anchor at one edge and a dead-end anchor at the other. Unbonded tendon profile in a two-way flat plate (section, not to scale) Stressing anchor (jack here) Dead-end anchor High point over column: tendon near top surface Low point at midspan Low point at midspan 9 in 30 ft column spacing 30 ft column spacing Span to depth: 30 ft x 12 = 360 in, divided by 9 in = 40 (PTI Technical Note 22, 2023 example) Placing tolerance: plus or minus 1/4 in in slabs 8 in or less, 3/8 in for 8 to 24 in (UH spec 03 38 00) Pull length: up to 125 ft stressed from one end, 250 ft from both ends (UH 03 38 00, CSU item 16)
The tendon drapes high over columns and low at midspan; a 9 in plate on 30 ft bays is a span-to-depth ratio of 40. Sources: PTI Technical Note 22 (2023), UH Section 03 38 00 (2018), accessed November 15, 2026.

Where you find them in commercial work: suspended floors in parking garages, office and hotel flat plates, and multifamily podium decks. The City of Seattle’s Director’s Rule 14-2014 credits the system with up to 40 percent less concrete and 75 percent less reinforcing steel than conventional framing, plus fewer construction joints and a lower building profile. The same mechanism appears in slabs on ground over expansive clay, covered further down.

How thick is a post-tensioned slab and how far can it span?

Published commercial examples put a post-tensioned flat plate at about 9 inches for 30 ft column bays, a span-to-depth ratio of 40 to 44. Heavy loads push the slab thicker: a food storage floor with live loads up to 600 psf used 14 inches plus drop panels. Ask your engineer for the governing span-to-depth ratio before fixing floor-to-floor heights.

Published exampleBaySlab thicknessSpan to depthSource
Typical office panel, PT flat plate30 x 33 ftAbout 9 in44 (33 ft x 12 / 9 in)PTI Technical Note 22, Section 9.1 (2023)
Same building with band beams (Fort Lauderdale, built from 2007)30 x 33 ft8 in slab, 17 in bands50 on the slab alonePTI Technical Note 22, Section 9.1
Research prototype, high-rise span30 x 30 ft, 7.5 ft cantilever9 in40PTI Technical Note 22, Section 10
Food storage facility, live load 100 to 600 psf29.7 x 29.7 ft14 in, drops to 31 in25PTI Technical Note 22, Section 9.2
Conventional flat plate, interior panel (contrast)28 ft clear span10.2 in code minimum33 on clear spanACI 318-19 Table 8.3.1.1
Slab thickness in published 30 ft bay examples vs conventional code minimumBar chart: PT slabs 8 to 9 in on 30 ft bays versus 10.2 and 11.2 in conventional minimums; heavy storage PT 14 in.inchesPT slab with 17 in band beams, 30 x 33 ft8PT flat plate, 30 x 30 ft prototype9PT flat plate, 30 x 33 ft office9Conventional flat plate, interior panel mi10.2Conventional flat plate, exterior panel wi11.2PT heavy storage, 29.7 x 29.7 ft with drop14.0
On 30 ft bays, published PT plates run 8 to 9 in against a 10.2 to 11.2 in conventional code minimum. Sources: PTI Technical Note 22 (2023), ACI 318-19 Table 8.3.1.1, accessed November 15, 2026.

PTI Technical Note 22 says its analytical examples use span-to-depth ratios slightly less than 45. CSU tells designers to meet or exceed Table 9.3 of the Post-Tensioning Manual, 6th Edition, and to switch from shear studs to column caps once slabs reach 10 inches. Garage decks exposed to deicing salt need at least 5,000 psi under ACI 318 exposure class F3, as our guide to concrete psi requirements explains.

What does ACI 318 require for a post-tensioned slab?

ACI 318, the concrete code adopted by the International Building Code (IBC), sets the minimum squeeze, tendon spacing and column integrity tendons for a post-tensioned slab. Owner specifications then add tighter limits on pull length, placing tolerance and stressing strength. The table lists the rules a reviewer checks first, with the clause behind each.

RuleValueSource
Average effective precompression, two-way slabs125 psi minimumACI 318 Section 8.6.2.1, cited in CSU item 3 and PTI TN 22
Practical precompression range150 to 175 psi optimum, 250 psi maximumCSU item 14
Integrity tendons through columnsShown on drawings; PTI notes a minimum of two tendons through the column each wayACI 318 Section 8.7.5.6.1 (CSU item 2); PTI TN 22
Uniform tendon spacingLesser of 8 times slab thickness or 5 ft (UH spec: 8h, max 54 in)CSU item 6; UH 3.1.D
Tendon encapsulationRequired; exposed strand details not permittedACI 318 Sections 20.6.3.1 to 20.6.3.3 (CSU item 1)
Pull length125 ft from one end, 250 ft from two endsUH 3.4.D; CSU item 16
Vertical placing tolerancePlus or minus 1/4 in (slabs 8 in or less), 3/8 in (8 to 24 in)UH 3.1.C
Cover to anchor wedge cavity2 in minimum at slab edgeUH 3.2.A.2
StrandASTM A416 low-relaxation, 270,000 psi ultimateUH 2.1.A
Broken tendons left unreplacedTotal force loss 2 percent maximumUH 3.4.H

How much force that means: at the 125 psi floor, one foot of a 9 inch slab (108 square inches) needs 13,500 lb of effective force, so a 30 ft wide panel needs 405,000 lb. One 1/2 inch strand of 0.153 square inches at 270,000 psi breaks at about 41,300 lb, so even at full ultimate strength it takes 10 strands; real designs carry more because effective force after losses sits well below ultimate.

StepInputResult
Area per foot of 9 in slab9 in x 12 in108 sq in
Force per foot at ACI minimum108 sq in x 125 psi13,500 lb
Force across a 30 ft panel13,500 lb x 30405,000 lb
Same panel at CSU optimum108 x 150 to 175 psi x 30486,000 to 567,000 lb
Strand breaking strength0.153 sq in x 270,000 psi41,310 lb
Strands at 125 psi if each carried its full ultimate405,000 / 41,3109.8, so 10 or more

When are the tendons stressed, and in what order?

Tendons in a commercial post-tensioned slab are stressed once field-cured cylinders show the concrete has reached the stressing strength on the drawings, at least 3,000 psi in the University of Houston specification, and within 3 to 5 days of the pour under the CSU guideline. Stressing early limits shrinkage cracking; stressing too early can crush concrete behind the anchors.

  1. Hold the pre-construction meeting. Seattle requires the general contractor, engineer of record, tendon placer, supplier, concrete supplier, finisher and testing agency; UH requires it at least 30 days before PT work starts.
  2. Inspect tendons and rebar before the pour. Seattle requires at least 4 hours between inspector sign-off and concrete placement, and at least two special inspectors on the pour.
  3. Cure test cylinders on the deck. Seattle Rule 13 bars using lab-cured cylinders to release stressing.
  4. Stress in sequence: temperature tendons, continuous slab tendons, added slab tendons, then beam and girder tendons (UH 3.4.F).
  5. Measure every elongation to 1/8 inch and send records to the engineer by the next working morning (Seattle Rules 16 and 17); UH accepts results within 7 percent of calculated.
  6. Cut tails 24 to 48 hours after engineer approval (Seattle Rule 18), at least 1/2 inch inside the concrete face (UH 3.5.A), then cap and grout the pockets.
  7. Close pour strips no sooner than 30 days after the second pour for plans up to 250 ft, or 60 days for larger plans (CSU item 8).
Post-tensioned slab stressing timeline From concrete placement to pour strip closure: stress at 3 to 5 days once field-cured cylinders reach the specified strength, cut tails 24 to 48 hours after engineer approval, grout pockets, close pour strips after 30 or 60 days. From pour to pour strip: when each post-tensioning step happens Day 0 Day 3 to 5 +24 to 48 h +24 h to 10 days 30 or 60 days Place concrete 2 inspectors on the pour (Seattle DR 14-2014); field-cured cylinders on deck Stress tendons At 3,000 psi or the EOR value (UH spec); within 3 to 5 days (CSU item 27) Approve, then cut Elongations within 7 percent (UH); cut tails 24 to 48 h after EOR approval (Seattle) Cap and grout Pockets grouted in 24 h (not encapsulated) or 10 working days (encapsulated) Close pour strip 30 days after 2nd pour if plan is 250 ft or less; 60 days if larger (CSU item 8) EOR = engineer of record. Lab-cured cylinders may not be used to release stressing (Seattle DR 14-2014, rule 13). Deck forms stay until the deck is poured and fully stressed; reshore at least 3 floors below (CSU item 28). Plans over 350 ft need a permanent expansion joint (CSU item 8). Sources: CSU Guidelines for Post-Tensioned Concrete Structures (2018); UH Section 03 38 00 (2018); Seattle DR 14-2014.
Stressing follows the pour by 3 to 5 days; pour strips stay open 30 days, or 60 days on plans over 250 ft. Sources: CSU guideline (2018), UH 03 38 00 (2018), Seattle DR 14-2014, accessed November 15, 2026.

Stressing is a federal safety item. OSHA 29 CFR 1926.701(c) keeps everyone except essential crew from standing behind the jack and requires signs and barriers around the stressing area. Seattle Rule 15 goes further and clears the deck of anyone not directly involved, because a tendon that breaks during stressing can cause serious injury. Curing strength gain by day is covered in our guide to concrete curing time.

Can you drill or core a post-tensioned slab?

Only after the tendons are located. CSU item 24 prohibits drilling into a post-tensioned slab unless tendon locations are marked, the slab has been x-rayed, or the tendons were photographed before the pour, and Seattle bars any drilling into the deck after placement. A cut tendon loses force over its full length, not just at the hole.

Because the drape runs from near the top over columns to near the bottom at midspan, no depth in the slab is automatically safe. The UH specification keeps tendons at least 6 inches from openings and limits horizontal sweeps to a radius of 480 strand diameters. CSU also limits shot pins to the concrete cover over the tendons and requires Schedule 40 steel sleeves, not PVC, near anchors.

Locating methodHow it worksRule or limitSource
Pre-pour photos or drone surveyPhotograph tendons on chairs before concrete covers themAccepted by CSU before drillingCSU items 24 and 29
Permanent slab markingPaint or inserts mark tendon bands on the soffitCSU asks for it where future changes are expectedCSU item 29
Ground-penetrating radar (GPR)Radar scan from one face, no radiationConfirm against shop drawings; no code depth standardIndustry practice
X-ray radiographySource on one face, film on the otherLicensed radiographers and a cleared area under NRC rules10 CFR Part 34

CSU item 18 calls de-tensioning a very dangerous operation and tells designers to avoid requiring it. If a renovation needs a new shaft or stair opening through a post-tensioned slab, budget a structural engineer to design the cut and re-anchoring; our structural engineer cost guide gives fee ranges.

Post-tensioned vs conventionally reinforced slab: which costs less?

A post-tensioned slab uses less concrete and steel, but adds strand, anchors, a stressing crew and inspection. At a 30 ft bay, the concrete saving against a code-minimum conventional flat plate is about 3.3 cubic yards per bay, worth roughly $0.62 per square foot at a 2026 public bid price. The larger savings are floor height and dead load.

FactorPost-tensioned slabConventionally reinforced slabSource
Thickness, 30 ft bayAbout 9 in10.2 in interior, 11.2 in exterior without edge beam (code minimum, 28 ft clear)PTI TN 22; ACI 318-19 Table 8.3.1.1
Concrete and rebarUp to 40 percent less concrete, 75 percent less rebarBaselineSeattle DR 14-2014
Crack controlPrecompression 125 psi minimum keeps slab in compressionRelies on bonded bars; see our rebar sizes guideACI 318 Section 8.6.2.1
ScheduleStress at 3 to 5 days; pour strips wait 30 to 60 daysNo stressing stepCSU items 8 and 27
Later penetrationsLocate tendons first; drilling prohibited without itScan for bars, cutting a bar is localCSU item 24
Special inspectionTendon placement, pour, stressing and cut-offRebar placement and pourSeattle DR 14-2014

Worked example for one interior 30 by 30 ft bay (900 square feet). The conventional thickness uses ACI 318-19 Table 8.3.1.1 for an interior panel without drop panels and 60,000 psi bars, clear span divided by 33, with an assumed 24 inch column. The concrete price is the $169 per cubic yard 4,000 psi low bid in Tioga County, NY (opened January 15, 2026), delivered material only.

LinePost-tensionedConventional
Clear span28 ft28 ft
Thickness9 in (PTI TN 22)28 x 12 / 33 = 10.2 in
Concrete per bay900 x 0.75 / 27 = 25.0 cu yd900 x 0.85 / 27 = 28.3 cu yd
Concrete cost at $169 per cu yd$4,225$4,783
Difference3.3 cu yd and $558 per bay, about $0.62 per sq ft, plus 1.2 in less height per floor

The ACI value is a minimum that lets designers skip a deflection calculation; a 30 ft conventional flat plate often ends up thicker or with drop panels, which widens the gap. For slab-on-ground pricing by thickness, see our concrete slab cost per square foot guide.

What does post-tensioned slab work cost in public bids?

We found no public bid tabulation or federal award that prices new post-tensioned slab work as a separate per-square-foot line; garages are usually bid as one structural package. Repair work is itemized: the City of Tampa’s June 22, 2021 garage repair bid priced broken tendon repair at $500 to $4,470 each across four bidders.

Item (Tampa bid 21-C-00036, Rivergate and other garages)UnitQtyBid rangeMedian of 4Median x 1.354 (2026)
Repair broken PT tendonsEach12$500 to $4,470$2,632$3,563
Repair PT tendon sheathingSq ft80$35 to $150$133$180
Re-grout PT tendon pocketsEach60$93 to $141$110$149
Post-tensioned beam repair (Rivergate)Sq ft25$175 to $288$206$278
Non-post-tensioned beam repair (Fort Brooke, contrast)Sq ft70$95 to $278$176$238
Unit price to repair one broken PT tendon, City of Tampa bid 21-C-00036Bar chart: broken PT tendon repair bids of $500, $1,763.33, $3,500 and $4,470 per tendon in Tampa, 2021.$ per tendonBid A500Bid B (low total bid)1,763Bid C3,500Bid D4,470
Broken tendon repair bids spread almost ninefold, $500 to $4,470 per tendon, in one 2021 Tampa garage contract. Source: City of Tampa bid tab 21-C-00036, accessed November 15, 2026.

The 1.354 factor is the change in the BLS producer price index for concrete contractors, nonresidential building work (PCU23811X23811X), from 145.919 in September 2021 to a preliminary 197.561 in September 2026. Quantities were small (12 tendons), so mobilization is likely spread into the unit prices; expect a single tendon call-out to cost more.

What should an owner inspect on a post-tensioned deck?

Post-tensioned slabs fall under the IBC special inspection program, and Seattle spells out the checkpoints: tendon placement, the pour, stressing, cut-off and pocket grouting. An owner or owner’s representative can ask for these records at each stage. Our special inspections guide covers who hires the inspector.

StageWhat to checkPass conditionSource
DeliveryMill certificates and 6 ft strand samples per shipmentSamples held by testing agency until final letterSeattle Rule 5
Before pourSheathing tears, chair spacing, profile heightsSupports at 4 ft maximum; repairs watertightUH 3.1.E and 3.1.G
PourSlump at chute, no added water beyond ticketTicket states gallons allowed per loadSeattle Rules 7 and 11
StressingCalibrated ram and gauge, one inspector per ramElongation within 7 percent of calculatedUH 3.4.C and 3.4.E; Seattle Rule 14
Cut-offTail length and capsCut 1/2 in inside face, capped within 24 hUH 3.5.A and 3.5.B
CloseoutPockets grouted, as-built tendon recordEngineer acceptance letter receivedSeattle Rule 4; CSU item 29

When is post-tensioning used for a slab on ground?

On expansive clay, IBC Section 1808.6.2 lets designers build a slab-on-ground foundation to the PTI DC10.5 standard or the WRI/CRSI method instead of deep foundations. The tendons tie the slab into one stiff mat that rides soil swell. The trigger is the expansion index in your geotechnical report; plasticity and swell values feed the design.

Residential contrast: house slabs use the same tendons, but warehouse rack, forklift and dock loads need their own design check.

Should your project use a post-tensioned slab?

Choose post-tensioning when column bays near 30 ft, a flat soffit and floor height matter, as in garages and podium decks. Choose conventional reinforcing when tenants will core the slab often and nobody will keep tendon maps. Long plans over 350 ft still work with a permanent expansion joint.

IfThenSource
Slab on ground over expansive soilDesign to PTI DC10.5 or WRI/CRSIIBC 2021 Section 1808.6.2
Supported bays near 30 ft, flat soffit wantedPrice a PT flat plate around 9 inPTI TN 22
Bays well under 30 ft and height is not tightPrice conventional; the code minimum may be close to PT thicknessACI 318-19 Table 8.3.1.1
Frequent future coring or anchorsPT only with marked or photographed tendons; else conventionalCSU items 24 and 29
Plan dimension over 250 ftAllow a 60 day pour strip delay in the scheduleCSU item 8
Plan dimension over 350 ftAdd a permanent expansion jointCSU item 8
Slab 10 in or thickerUse column caps, not shear studsCSU item 26
Post-tensioned or conventional slab decision flowchart Four questions route a commercial floor to a post-tensioned flat plate, a conventionally reinforced slab, or a post-tensioned slab with mandatory tendon mapping. Commercial floor or slab to frame Slab on ground over expansive soil flagged by the geotechnical report? Yes Design to PTI DC10.5 or WRI/CRSI (IBC Section 1808.6.2) No Elevated bays near 30 ft, flat soffit, floor-to-floor height or weight matters? No Price a conventionally reinforced slab (ACI 318 Table 8.3.1.1 minimums) Yes Will tenants core or anchor into the deck often (labs, retail turnover)? Yes PT only with as-built tendon maps or slab marking (CSU item 29) No Building plan longer than 350 ft in one direction? Yes PT with a permanent expansion joint (CSU item 8) No Post-tensioned flat plate: about 9 in for 30 ft bays (PTI TN 22) Pour strips: 30 day delay up to 250 ft, 60 days above (CSU item 8). Engineer of record makes the final call.
Four questions route a commercial floor to PT or conventional framing; a 9 in PT plate fits 30 ft bays. Sources: IBC 1808.6.2, ACI 318-19, CSU guideline (2018), PTI TN 22, accessed November 15, 2026.

Before fixing a garage column grid against the 30 ft PTI examples, check stall and aisle sizes in our parking space dimensions guide.

What do common guides get wrong about post-tensioned slabs?

Several page-one guides were written for houses or for markets outside the U.S. and carry numbers that do not fit a commercial post-tensioned slab. The table sets three claims against the primary document.

What a guide saysWhat the primary source saysSource
A top-ranking general guide says concrete cures 20 to 25 days to reach 75 percent strength before stressingStress within 3 to 5 days, once field-cured cylinders reach the specified strengthCSU item 27; UH 3.4.B
Residential guides cite stressing at 2,000 psiCommercial owner spec: not less than 3,000 psi unless drawings say otherwiseUH 3.4.B

Slab design starts from the soil bearing capacity in the geotechnical report and the vapor barrier under the slab.

How we compiled this

We read 7 primary documents in November 2026: PTI Technical Note 22, the CSU Seismic Review Board post-tensioning guideline, the University of Houston Section 03 38 00, Seattle Director’s Rule 14-2014, OSHA 29 CFR 1926.701, the City of Tampa bid tab 21-C-00036 and the BLS PPI series, plus the Tioga County bid already used on our site. ACI 318-19 and IBC clauses are cited as quoted in those documents or from the code tables. We did not test, design or price any slab ourselves.

Frequently asked questions

How thick is a post-tensioned slab in a parking garage?

Published examples put a post-tensioned flat plate at about 9 inches for 30 ft column bays, a span-to-depth ratio of 40 to 44 (PTI Technical Note 22, 2023). Band-beam layouts can drop the slab to 8 inches with 17 inch bands. Heavy storage loads pushed one 29.7 ft bay to 14 inches with drop panels. Your engineer sets the final thickness from loads and fire cover.

How long after pouring are post-tensioned tendons stressed?

The CSU post-tensioning guideline requires stressing within 3 to 5 days of the pour to limit shrinkage cracking. The release is strength, not days: the University of Houston specification requires at least 3,000 psi unless the drawings say otherwise, and Seattle Director’s Rule 14-2014 only accepts field-cured cylinders, never lab-cured ones, to prove that strength.

Can I drill into a post-tensioned slab to install an anchor?

Not until the tendons are located. CSU item 24 prohibits drilling unless tendon locations are marked, the slab is x-rayed, or pre-pour photos exist, and it limits shot pins to the cover over the tendons. Tendons run near the top over columns and near the bottom at midspan, so no depth is automatically safe. Ask the owner for the as-built tendon drawings first.

What happens if a tendon is cut?

An unbonded tendon loses its force along its whole length, not just at the cut, because the strand is greased and free inside its sheath. The University of Houston specification limits unreplaced broken tendons to 2 percent of a member’s total prestress force. In a 2021 City of Tampa repair bid, replacing one broken tendon was priced from $500 to $4,470.

Is a post-tensioned slab cheaper than a conventional slab?

It uses less material: Seattle Director’s Rule 14-2014 cites up to 40 percent less concrete and 75 percent less reinforcing steel. At a 30 ft bay, the concrete saving against a code-minimum conventional flat plate is about 3.3 cubic yards per bay, roughly $0.62 per square foot at a 2026 Tioga County bid price, before strand, anchors and stressing labor.

What is the minimum precompression in a post-tensioned slab?

ACI 318 Section 8.6.2.1 requires an average effective precompression of at least 125 psi in two-way post-tensioned slabs. The California State University guideline treats 150 to 175 psi as optimum and caps flat plates at 250 psi. For a 9 inch slab, 125 psi equals 13,500 lb of effective force per foot of width.

Sources

Last reviewed November 2026 by the CB&C Editorial Team. See our editorial standards.

← Back to all articles